Brand Name : HAOLISEN
Model Number : HR-4000BLB
Certification : IATF16949 , ISO9001
Place of Origin : Shanghai China (Mainland)
MOQ : Negotiation
Price : Negotiation
Supply Ability : 200 Tons Per Day
Delivery Time : 30-60 Days
Packaging Details : 50kg、60 kg、200kg、1000kg packaging barrels
main ingredients : Organic acid
Performance : film is uniform
Application field : Bicycle parts
Cooperation case : GLANT
Special Bicycle white electrophoresis paint
HR-4000BLB Epoxy acrylic Color Cationic Electrocoat is HLS Paint (Shanghai) Co., Ltd., the eighth generation of independent research and development of electrophoretic coating. This coating by epoxy acrylate modified, the film also has excellent corrosion resistance and weatherability, smooth appearance and full, suitable as a base topcoat system. In addition, the lead, cadmium, chromium, mercury and other heavy metals, two-component, water dispersible resin, at the same time, previous generations of the product characteristics, have good adaptability to the galvanized steel, almost can be applied to all metal coating, such as: cold hot rolled steel, galvanized steel, aluminum, zinc Aluminum Alloy plate, stainless steel plate.
1, The bath has strong anti-shrinkage and anti-pollution ability
2, Good stability of bath can adaptable for a longer updating cycle
3, Coating fullness of good, better substrate hiding
4, Strong anti-corrosion propertie
1, Curing agent: totally enclosed multi-isocyanates
2, Solvent: alcohol ether
3, Pigment: Titanium pigment, Organic pigment, kaolin, antirust pigment
Filling tank proportion and method :
⑴ Bath preparation
Ratio:
Resin 1400.00
Paste 233.00-175.00
DI water 1785.00
Total 3418.00-3360.00
⑵ Ripening conditions
Sample quantity: 3000~3500g
Container: 5L (Diameter 16cm)
Tank temperature:28-30 ℃
Time: 24~48Hr
Mixed conditions: impeller diameter 8cm (speed 200rpm)
(3) Coating conditions
Experimental panel: phosphated cold-rolled steel plate
Tank temperature: 28-35℃
Pole ratio: A/C = 1/2 ~ 1/4
Distance of electrodes: 15cm
ED time: For full immersing 1-3 minutes ( 20 seconds soft start)
Baking conditions:(165-185)℃×(20-30)min (Keeping temperature of parts coated)
Construction equipment
Cathodic electrophoretic coating construction in the electrophoresis tank, so need to have the following equipment:
Electrophoresis tank
Circulation devices (including filter, fill the paint device)
DI water equipment
DC power supply and the power supply unit
Anode box (tube) and circulation device
Ultrafiltration device
Cleaning devices
Heat exchanging equipment
Curing device
![]() |